Swimming is an enamel paint pvc for pools made of soft PVC, semi-flexible and rigid materials , polycarbonate and plastic. Swimming paint pvc with harmonizing effect , consolidates the media and regenerates them . The product mix is made with the highest quality resins schell long filament bundles that smooths and compacts the surface. Swimming paint PVC, ideal for the recovery of lean ground swimming pools , outdoor pools with traditional support structures and welded sheets thesis . Swimming pvc paint is the ideal solution, an excellent product for the recovery of degraded PVC swimming pools and various plastics.
YIELD TO M ² KG . 7-8
DILUTION: Thinner for PVC at 10 % or less ( or nitro solvent ' )
GLOSS : Gloss 45
DRYING : very fast. Dust free 120 minutes , in depth 24 hours, complete 5 days
CYCLE: apply one coat ( Recommended )
Fill tank : 8/10 days
Aging of the plastic sheet : the classic PVC coating after a few years older or worn , creating stains and spots in patches more and more ' big and it varies its pleasing appearance . Also the continued use of chlorine , contributes to aging of the fabric , creating wear with residues of dust , alkaline deposits , lines of residues stagnant on the towel . The formation of lichen attached on the bottom of the ammalorano .
PVC loses color and crosslinks losing its natural texture . Our cycle provides for the recovery and prolongation of life and avoid high costs of replacement of the cloth .
Swimming paint PVC is a product based on biphenyls, neanderthal, precious pigments , fillers and special additives that micronized together in an exclusive formula affect the following features of recovery of the cloth :
high corrosion resistance , excellent resistance to sea water and chemical agents ; exceptional weather resistance , Swimming paint PVC version is ideal for painting swimming pools plastic , PVC, and pexiglass FIBERGLASS , for the use of water tanks not drinking , bathing pools and any other object that is to be immersed in water or contain it. The concentrated formulation has a drying particularly suitable for PVC substrates , resin plastic and rubber contained differentiates it alive for its good adhesion to the substrate . Do not puff , his particular mesh fibered and filamentous makes it unique and suitable for the extension of the life of the sheets even after their natural decomposition and aging. The special adhesion is observed within the application. The plastic filament voltage conforms to the support by joining with extreme force .
Test compatibility of accession: it is advisable to do an adhesion test prior to painting the entire pool . The various problems of aging of the cloth or PVC support if very degraded, may be incompatible accession. If the sheet is already being started wearing down the anchor will have problems , then subject to periodic restoration .
Directions for use:
Can be used for external for the waterproofing of tanks , as a final coating , for swimming pools or for finishing high chemical resistance for iron structures in very aggressive conditions . Not suitable for coating containers designed for drinking water and food in general .
After painting wait its stability , at least , 5/10 days before filling the same with water .
Colors : We recommend that the annual maintenance to apply the color of the same shade of color of the cloth . Application by airless spray , roller such as mohair short-haired . Spread out a hand full bodied and well coated to avoid lumps of paint. Any shooting or retouching, or only after 36/48 hours away from the first hand. Be careful, once applied paint pvc swimming not use any robot that compromise the durability. Do not sow chlorine by hand but follow only chlorination with skimmer.
duration:
IT IS RECOMMENDED THAT A HAND PAINT FOR SEASON
Mixture and composition of the product : Swimming PVC paint is composed of a mixture of extracts of resins that can not be changed . It recommends its scrupulous method of application and mixing as it is a compound for balanced adhesion , resistance , color and thickness .
A poor mixing or dilution may result in loss of the characteristic and the decline in stability and anchoring .
It is recommended to strictly follow the procedure recommended by the manufacturer data sheet .
THINNER : MUST USE THE SUPPLIED DILUENT FROM HOME , OR FOR THINNER PVC chlorinated rubber ' , NOT' COMPATIBLE WITH OTHER SOLVENTS .
Il ciclo prevede poi una manutenzione periodica in quanto l'invecchiamento del telo in pvc tende a perdere consistenza. Le note tecniche ed i consigli sono frutto di esperienza del nostro laboratorio e dei nostri test. Non possiamo assumere responsabilità su cantieri dove non si rispettano i nostri consigli e non seguiti dai nostri tecnici di fiducia.
Nota per l’utilizzatore:
Le informazioni contenute in questa scheda si basano sulle conoscenze disponibili presso di noi alla data dell’ultima versione. L’utilizzatore deve assicurarsi della idoneità e completezza delle informazioni in relazione allo specifico uso del prodotto. In caso di lavorazione dei nostri prodotti, sarà il cliente stesso ad assumersi la responsabilità del rispetto di tutte le norme di legge e sicusezza. Si consiglia di abilitare i cantieri dopo i controlli del direttore dei lavori che ne determina l'abilitazione e la sicurezza per l'uso pubblico.
Non si deve interpretare tale documento come garanzia di alcuna proprietà specifica del prodotto. Poichè l'uso del prodotto non cade sotto il nostro diretto controllo, è obbligo dell'utilizzatore osservare sotto la propria responsabilità le leggi e le disposizioni vigenti in materia di igiene e sicurezza. Non si assumono responsabilità per usi impropri.